Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. |
Omnia Plastica Akulon® PA 66 - Akulon 66 - Dry Polyamide obtained by the polymerisation of Hexamethylenediamine and Adipic acid. It is one of the oldest engineering plastics, having been created in the USA in 1930. Due to its origin it is widely.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous; 5,000 h |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous; 5,000 h |
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B650 Mi10 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B650 Mi10 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | |
Abatron 440 A/B Filled Potting Compound
(discontinued **) Black or color dielectric hard casting adhesive room temperature epoxy. 100/20 ratio.Information provided by Abatron. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL B63 SG 10 Nylon 6 for injection molding, 10% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Pressed Bushings |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | 5000 hours; 50% Tensile Strength; IEC 216; DIN 53446 |
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6) at 50% RH Zellamid® 250 is noted for its high temperature resistance and high tensile strength. It is the hardest and most rigid type of extruded Nylon. Main characteristics are high resistance to fuels, oil.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSI 740 Polystyrene Polystyrene 740 is an impact polystyrene designed for extrusion and injection molding. It is especially suitable for extrusion thermoforming applications requiring high glass and high stiffness, suc.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | |
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Deflection Temperature with load unspecified |
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod Red color. Turcite® TX is engineered to handle moderate load, high speed applications. It exhibits an excellent surface finish when machined. It has a long service life and exceptionally low coe.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Wet Service |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Wet Service |
Chesterton ARC MX1 Vertical Build Extreme Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”).. |
|||
Maximum Service Temperature, Air | <= 95.0 °C | <= 203 °F | Laundering Resistance |
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 CM-RS EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 F-7142 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Wet Service |
Chesterton ARC MX2 High Wear Fine Particle Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Wet Service |
Chesterton ARC MXC Castable Extreme Wear Compound Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | short term; EMS |
EMS-Grivory Grivory® TR 90 LXS PAMACM12 Product description: Grilamid TR 90 LXS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LXS natural contains a processing.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 CM-HD EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 CM-KPA 45 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 CM-S EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Permanent |
3M ScotchCal™ 3690E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Permanent |
3M ScotchCal™ 3698E Graphic Film Material 3M™ ScotchCal™ Graphic Film Materials 3690E and 3698E are flexible cast vinyl films suitable for conforming to curved and textured surfaces, including most low surface energy plastics and small di.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | Long Term |
CENTROPLAST CENTROMID 12 Polyamide 12 This extruded material has good impact resistance, low moisture absorption and good chemical resistance. It is used in precision elements, drive parts, cases and housingsInformation provided by CEN.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | short term; EMS |
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c.. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | ASTM D 3575 |
Eurofoam Porocell POR 304 CM-GR EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Maximum Service Temperature, Air | 95.0 °C | 203 °F | short term; EMS |
EMS-Grivory Grivory® TR 55 LY PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c.. |