Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries 306 Surface Insensitive Instant Superglue Low viscosity for difficult to bond rubber compounds |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries 354 Surface Insensitive Instant Superglue Gel for porous, hard to bond surfaces - large gap |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
ND Industries SuperGlue Ethyl 322 High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE 2000CP FLUORESCENT Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE FLUORESCENT advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performan.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 110 (5 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (500 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 150 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 115 (20 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 130 CLEAR FLEXIBLE (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 440 - GEL BLACK TOUGHENED advanced thixotropic formula is designed to polymerize instantly by absorbing surface .. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 143 BLACK TOUGHENED (300 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 143 – BLACK TOUGHENED advanced formula is designed to polymerize instantly by absorbing surface moisture. The p.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives TURBO FUSE SERIES 180 BLACK TOUGHENED (2400 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 440 - GEL BLACK TOUGHENED advanced thixotropic formula is designed to polymerize instantly by absorbing surface .. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Cured State |
Palm Labs Adhesives Turbo Fuse Series 190 (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Garlock 2103 C.I. SBR/NBR Sheet Rubber, Polyester Insert Garlock cloth-inserted materials are designed to add stability where mechanical fastening is necessary, and to reduce gasket creep where heavy flange loading is required.Style #2103 C.I. is a smooth.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | dry |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | dry |
ITW Devcon Rubber Repair / Castable Urethane Cable Cast FR, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Spartech Polycast UF4 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Saint-Gobain Norton® V990 Poly Liner Pressure Sensitive Adhesive Foam Sealant Description: Closed cell PVC foam with a pressure-sensitive adhesive on both sides. Proven Performance: Norseal® V980/V990 foam sealant combines a closed cell polyvinyl chloride foam substrate wt.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous Use |
Westlake Plastics Propylux® Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance it abrasion. These properties makes it suitable f.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Continuous |
Trelleborg Sealing Solutions HiMod® 912 Thermoplastic Bearing Thermoplastic BearingCharacteristics: HiMod® 912 was developed for application with intermittent temperature of 200°F, but requiring a more demanding bearing material with higher performance, imp.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® 420 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Permabond 792 Cyanoacrylate, Surface insensitive PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Maximum Service Temperature, Air | 82.2 °C | 180 °F | |
Loctite® 416 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |