Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 65.6 °C | 150 °F | |
Alcoa KAMA 4100 Prime APET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | |
Alcoa KAMA 4200 RPET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | |
Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Upper limit of working range |
Heatbath/Park Parquench 60 Water-Based Quenchant The lower molecular weight polymer package. It is generally used for lower alloy steels, castings, forgings and most aluminum applications. Typical concentration is 15%.Information provided by Hea.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Upper limit of working range |
Heatbath/Park Parquench 90 Water-Based Quenchant The higher molecular weight polymer package. It is generally used for higher alloy steels and all types of metals where the control of distortion is of prime importance. Typical concentration is 15.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Upper limit of working range |
Heatbath/Park Polyquench 10 Water-Based Quenchant Solution of relatively low molecular weight organic polymer, corrosion inhibitors, biocide and anti-foaming agent. The polymer is inversely soluble above 160°F. Typical concentration is 15%.Info.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Upper limit of working range |
Heatbath/Park Polyquench 20 Water-Based Quenchant Water solution of standard, "Type I", polyalkylene glycol quenchant. The polymer is inversely soluble above 1650°F. Typical concentration is 15%.Information provided by Heatbath Corporation - Pa.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Upper limit of working range |
Heatbath/Park Polyquench 15 Water-Based Quenchant Water solution of organic polymer, corrosion inhibitors, biocide and anti-foaming agents. The polymer has normal solubility and greater washability than other synthetic quenchants. Typical concentr.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | ASTM D1329 |
Seals Eastern 7336 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | ASTM D1329 |
Seals Eastern 7344 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | ASTM D1329 |
Seals Eastern 7345 Highly Saturated Nitrile Rubber HNBR for Oil & Gas serviceInformation provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Martens Dimensional Stability |
CMT Materials PROTOBLOCK Air Permeable Prototype Tooling Material PROTOBLOCK is a new composite material made of inorganic granules and epoxy resin engineered to form a micro-porous structure for use as prototype vacuum form or thermoform tooling. The material is.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | |
Bostik 2385 General Purpose EVA Glue Stick Bostik 2385 General Purpose EVA Glue StickGood general purpose bonding of paper, wood, cardboard, foam and fabrics. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Long Term |
3M 9832 Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Application |
3M Scotchrap™ 50 Tape 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Application |
3M Scotchrap™ 51 Tape 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Long Term |
3M 9832HL Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | Upper limit of working range |
Heatbath/Park Speed Quench #1 Water-Based Quenchant An inhibited "brine" quench supplied in granular form to be dissolved in water. While quenching like brine or caustic, it prevents rusting and does not generate disagreeable fumes. Recommended conc.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | |
Bostik 2105 Low viscosity, short open time EVA Glue Stick Bostik 2105 Low viscosity, short open time EVA Glue StickLow viscosity. Short open time for woodworking and packaging applications. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | |
Alcoa KAMA 4203 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |
|||
Maximum Service Temperature, Air | 65.6 °C | 150 °F | |
Alcoa KAMA SealPET™ 4205 RF Sealable RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |