Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 525 °C | 977 °F | |
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded .. |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
GrafTech GRAFOIL® GHL Standard Fluid Sealing Grade GHL Laminate GRAFOIL® Grade GHL is a laminate made with GRAFOIL® Grade GTB flexible graphite. Laminate thicknesses > 0.060" will be adhesively bonded to final thickness. Laminate thicknesses |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden.. |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall.. |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu.. |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â.. |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
Alliance A-5 Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
Alliance A-5-7 Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
Alliance A-5DG Alnico Magnetic Material |
|||
Maximum Service Temperature, Air | 525 °C | 977 °F | |
Alliance A-6 Alnico Magnetic Material |