Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 52.0 - 64.0 °C | 126 - 147 °F | HDT |
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Wet Service (Intermittent) |
Chesterton ARC CS4 low-viscosity, 100% solids, barrier coating Description: An advanced composite formulated to protect concrete surfaces from harsh chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat in a 2 coat syst.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Wet Service (General) |
Chesterton ARC PW Potable Water Coating Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Wet Service |
Chesterton ARC S1 General purpose coating Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Wet Service |
Chesterton ARC S2 Ceramic reinforced erosion resistant coating Description: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% soli.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | |
3M 665 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | |
3M 666 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | |
3M 9425 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ5208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ5832 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ6216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | for up to 30 mins, removes cleanly |
3M Scotch® 250 Flatback Masking Tape Scotch® Flatback Masking Tape 250 is used for bundling and holding applications where a stronger paper backing is needed.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M SJ5201 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M SJ5300 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M SJ6100 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M SJ6344 Protective Product, Molded Shapes 3M Bumpon Protective Products SJ6344 is a pressure-sensitive adhesive-backed, molded polyurethane product. The Bumpon SJ6344 is called an Easy Slide Series because it incorporates a special abrasion.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ6208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ6232 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Application |
3M SJ5202 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Maximum Service Temperature, Air | 52.0 °C | 126 °F | Wet Service |
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating An advanced composite formulated to protect concrete and metal surfaces from corrosion and chemical attack. It is normally applied at a thickness of 1-2 mm (40-80 mils) per coat. However, greater si.. |