Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat resistance per ASTM D794 |
Plenco 7466 Phenolic, Nodular, Injection Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 2308 Phenolic, Granular, Transfer Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 3509 Phenolic, Granular, Transfer Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 4414 Phenolic, Granular, Transfer Molded PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional .. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 4300 Phenolic, Granular, Compression Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 4466 Phenolic, Granular, Transfer Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 4485 Phenolic, Granular, Injection Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 5118 Phenolic, Granular, Transfer Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 7507 Phenolic, Granular, Transfer Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 4300 Phenolic, Granular, Transfer Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Maximum Service Temperature, Air | 203 °C | 397 °F | Heat Resistance; ASTM D570D |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |