Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 179 °C | 354 °F | Short Term |
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **) ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc. |
|||
Maximum Service Temperature, Air | 179 °C | 355 °F | Intermittent |
Ensinger Tecamid® MDS® Molybdenum Disulfide Filled Nylon (PA) Tecamid MDS® has enhanced surface lubricity and wear resistance over unfilled nylon. It is an ideal material to replace metals in machinery. Low surface friction Increased surface hardness Incre.. |
|||
Maximum Service Temperature, Air | >= 179 °C | >= 355 °F | Temperature Index |
AlphaGary Megolon™ HF 8142 UV Low Smoke Halogen Free 105°C Rated HFFR Jacket and Buffer Compound. UV resistant. Application examples include Data Cables, Optical Cables. |
|||
Maximum Service Temperature, Air | >= 179 °C | >= 355 °F | Temperature Index |
AlphaGary Megolon™ HF 8142 Low Smoke Halogen Free 105°C Rated HFFR Jacket and Buffer Compound. Application examples include Data Cables, Optical Cables. |