Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AC 80-5 Dense Refractory Brick Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 85-10 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 85-5 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast AC 90-8 Dense Refractory Brick Description: Excellent resistance against alkali- and metal slags. The 8% chromium-oxide addition gives good volume stability at very high temperatures. Applications: chemical incinerators, combusti.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast CURON 170 GM Dense Refractory Castable Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation under load - t<sub>a</sub> |
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
ICE Al2O3 94 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast AK 70 KP Dense Refractory Brick Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics VELCRETE G403 Gunning Castables Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sharadaa Ceramics ZAP 007 Smart Cast Application Special Properties: Hot abrasion, Wear resistanceIndustry: SteelApplication: False Chute, Tundish BackupInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ SL-150 Hollow Spheres EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Sapco 98% Aluminum Oxide Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Continuous |
Unifrax Fibermax® Duraboard® 17H Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Continuous |
Unifrax Fibermax® Duraboard® 17R Board Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. .. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | |
Zircar Zirconia BusterF Alumina Bulk Fiber Insulation Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rig.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | Intermittent |
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | No Load |
CoorsTek AD-96 Alumina (nom. 96% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
Chosun Refractories LPCT-17PI Lance Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
Chosun Refractories SFC-70R High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1700 °C | >= 3090 °F | |
China-Yixing Longly Refractories Plate Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Maximum Service Temperature, Air | >= 1700 °C | >= 3090 °F | |
China-Yixing Longly Refractories Zirconia Ceramics LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,.. |
|||
Maximum Service Temperature, Air | 1700 °C | 3090 °F | no load |
Astro Met AmAlOx 68 Alumina - Aluminum Oxide General Description:AmAlOx 68 alumina (Astro Met Aluminum Oxide) is a high purity 99.8% aluminum oxide (alumina) ceramic which has been developed and optimized for maximum wear resistance and corros.. |