Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Ritelok GM18 Aluminum Parts Gasket Maker Anaerobic. Flexible gasket maker for aluminum flanges. Replaces pre-cut gaskets, Does not shrink or relax, flexible, Withstands temperatures from 65°F to 300°F (55°C)-150°C), .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
ND Industries 533 Retaining Compound High strength sealing applications for non migration material |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Cured |
Parker Chomerics Tecknit® 72-08116 Silver-Filled Epoxy System Description: This is a silver filled epoxy system designed for maximum performance and lowest volume resistivity. It is easily mixed 1:1 by volume or weight, from the two one-ounce jars. Its consist.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Permabond LM113 Anaerobic Threadlocker Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Continuous |
Garlock Klozure® Mill-Right® ES HNBR Oil Seal A proprietary formulation of Hydrogenated Nitrile (HNBR). Engineered specifically for high-performance applications that demand the tightest sealing system, longest service life, and constant opera.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | continuous |
Lucas-Milhaupt Silvalite Brazing Alloy SILVALITE is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on v.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Master Bond EP62-1 High Glass Transition Temperature Epoxy System Master Bond EP62-1 is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. The cured epoxy resin ex.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 3105 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 3491 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Hexcel® HexWeb® HRH-10/F50 - 4.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 638 Maximum Strength Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Continuous |
Ensinger XP-46 Compression Molded Unfilled PCTFE PCTFE is a high performance crystalline polymer with excellent chemical resistance. Because of its low moisture absorption, PCTFE can operate in a continuous service temperature of -250°F to 300°F.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
DuPont Teijin Films Mylar® MDA Polyester Film, 750 Gauge Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
3M Scotch-Weld™ GM18 Gasket Maker Anaerobic Adhesive 3M™ Scotch-Weld™ Gasket Maker Anaerobic Adhesives are one-component anaerobic sealants formulated to replace pre-cut gaskets or used as form-in-place gaskets that cure at room temperature and seal.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | up to 30 mins |
3M 2497ST High-Temperature Tear Resistant Polyester Tape 3M™ High-Temperature Tear Resistant Polyester Tape 2497ST is designed for use in masking applications where sliver resistance and clean removal are required.Information provided by 3M |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
3M 425 Aluminum Foil Tape 3M™ Aluminum Foil Tape 425 is a 5 mil nominal dead soft aluminum foil backing combined with a transparent acrylic adhesive.Information provided by 3M |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
3M 427 Aluminum Foil Tape 3M™ Aluminum Foil Tape 427 is a 5 mil nominal dead soft aluminum foil backing combined with a transparent acrylic adhesive. 3M aluminum foil tape 427 offers an easy-release liner.Information provid.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Short term |
3M 4411G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Service |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Service |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Service |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Short term |
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP 3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Long Term |
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Saint-Gobain Furon®, Kapton® K275 Tape Description: A 1 mil thermally conductive Kapton® film, coated on both sides with 2 mils of thermally-conductive pressure-sensitive adhesive. Recommended uses: Excellent for use in small, compact e.. |