Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek J-1 Ropes Available in braided or twisted form. Excellent tensile strength and abrasion resistance. Low thermal conductivity.AdvantagesExcellent Abrasion Resistance Fair Compression and Recall Information p.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek Pyrite Vacuum Formed Product Off White ColorApplicationsTap hole cones Riser sleeves Launder insulation Head boxes Ladle lining Pouring cups AdvantagesGood thermal shock resistance High strength/weight ratio Low thermal conduct.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek M-9 Fiberseal Blanket Maxsil ceramic-free insulation with excellent chemical resistance. Shot free.Dimensions889 mm x 24.4 m x 13 mm889 mm x 11.9 m x 25 mmApplicationsBlankets Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Operating Temperature |
Hoskins Manufacturing Chromel® Thermocouple Wire Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usageChromel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsu.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Short term |
Mid-Mountain Materials SILTEX® 1800 Amorphous Silica Industrial Textile SILTEX® 1800 is a family of high performance textiles comprised of high purity, high strength amorphous silica fibers. SILTEX® 1800 Industrial Textiles demonstrate excellent thermal stability,.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Upper limit of working range |
Heatbath/Park High Speed 60 High Speed Hardening Salt Solution Treating Salt. A neutral salt designed for heat treatment high alloy steels requiring temperatures of 1650° to 2200°F. Formulated per MIL-S-10699-B, Class 6.Information provided by H.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Upper limit of working range |
Heatbath/Park High Speed 60 Neutral Salt A neutral salt designed for heat treatment high alloy steels requiring temperatures of 1650° to 2200°F. Formulated per MIL-S-10699-B, Class 6.Information provided by Heatbath Corporation - Par.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Sharadaa Ceramics And Bulk Fiber Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Lo-Con™ Felt Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Recommended Operating Temperature |
Unifrax Foamfrax® Isofoam Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites RS-201 Refractory Sheet ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Chosun Refractories 1260BULK Bulk Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Chosun Refractories 1260PAPER Paper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Normal oxidizing atmosphere |
BNZ Materials BNZ-23A Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Normal oxidizing atmosphere |
BNZ Materials C-22 Z Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
BNZ Materials Bazelite 2300 LI Insulating Castable Blaz 2300 L is similar to Blaz 2300 but suitable for those applications where reducing conditions might be encountered. These high purity, low iron products are specifically designed for both back-u.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Aremco Pyro-Paint™ 634-AS1 High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Duraset® Flet Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek Fiber Seal Y-1 Ceramic fiber paper Y-1 Fiberseal paper is a light-weight refractory material. Y-1 is resistant to most chemicals with the exception of hydrofluoric and phosphoric acids and strong alkalis.ApplicationsGaskets Seals Sp.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Sinotek Materials LG Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek M-1 High-Temperature Felt A light-brown material.Dimensions483 mm x 7.6 m 13 mm thickApplicationsHigh-temperature gasketsInformation provided by Pyrotek. |