Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 260 °C | 500 °F | Reducing Atm. |
SGL Carbon Group EK 201 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 260 °C | 500 °F | Reducing Atm. |
SGL Carbon Group EK 2201 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 260 °C | 500 °F | Reducing Atm. |
SGL Carbon Group EK 2241 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 260 °C | 500 °F | |
Arlon 920-10Bxx-P0 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Maximum Service Temperature, Inert | 260 °C | 500 °F | |
Arlon T1020-R004-## 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number.Desi.. |