Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 10502R125 Cured/Post-cured, Unsupported Silicone Rubber
Product Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silic..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 10842S085 Fully Cured, Unsupported Silicone Rubber
Product Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by AR..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 10842S125 Cured/Post-cured, Unsupported Silicone Rubber
Low ModulusProduct Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information pro..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as ..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 30400N085 0.085" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51422R020 0.020" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and should no..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material ..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material ..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production materi..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 99202R010 0.010" Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should no..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 99410R015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Design/Construction:Interleave: 0.001" FEPSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and sho..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 99570R010 0.010" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon CP-RC-3918 Silicone Bulk Compound
This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon R32390B020 0.020" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassAll ingredients of product are listed in 21 CFR 177.26000This data represe..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 41940C020 0.015" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51163X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber50" wideThis data represents typical values for the production material and should not..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51224R015P 0.015" Semi-cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Semi-cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and shou..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51426R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51561R015 0.015" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the ..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 51986RA020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the producti..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate
0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number...
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and ..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET
Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use..
Maximum Service Temperature, Inert 232 °C
450 °F
Arlon 48576R006 0.0055" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Uncured RubberSubstrate: Prime Coated 1080 FiberglassSide 2: Uncured RubberThis data represents typical values for the production mater..