Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group EI 2100 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group EK 200 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group EK 2200 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group EK 2240 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group Ridurid® EK 60 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group Ridurid® V 1017 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | Reducing Atm. |
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 18986XA023 0.023" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 32980XA015 0.015" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 51981XA015 0.0150" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil PolyethyleneThis data r.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 910-10Rxx-P1 0.010" Cured, Self-Fusing Silicone Rubber 1.0 inch wide, 0.010" thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 920-10CxxFR-P1 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, brown, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 920-10Hxx-P0 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.D.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 930-10Rxx-P1 0.030" Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 99322B015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Static dissipating siliconeDesign/Construction:Interleave: 0.0025" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Chemlock 607This data repres.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon LW301Bxx-P0 0.030" Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Des.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon LW40125B12-P0 0.040" Self-Fusing Silicone Rubber Tape 1.25 inches wide, 40 mil thick, black, triangular cross-section, self-fusing silicone tape. Product is supplied in 12 yard long roll lengths.Design/Construction:Rubber: Cured Self-fusing Silicone R.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon R34710R020 0.020" Uncured Silicone Rubber with Mylar Carrier 20 mil thick, uncured, uncatalyzed silicone rubber. Used for sealing biochemical reaction chambers.Design/Construction:Liner: 3 mil Pink PEProduct: Uncured Silicone RubberCarrier: MylarThis data.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | |
Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | |
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Maximum Service Temperature, Inert | 204 °C | 399 °F | |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 44571XB015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate) Side 2: Uncured Silicone RubberInterleave: 2.5 mil .. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 915-20Hxx-P0 0.015" Self-Fusing Silicone Rubber 2 inch wide, 15 mil thick, pale yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part num.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon T1012-R004-xx 0.012" Self-Fusing Silicone Rubber Tape 1 inch wide, 12 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |
|||
Maximum Service Temperature, Inert | 204 °C | 400 °F | |
Arlon 32570XA020 0.020" Uncured Silicone Rubber on Polyester Film Carrier Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |