Maximum Service Temperature, Inert 1500 °C
2730 °F
Inert/Vacuum
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Maximum Service Temperature, Inert 1500 °C
2730 °F
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
DN 70 is a ZTA Alumina Toughened Zirconia.
Maximum Service Temperature, Inert 1500 °C
2730 °F
CeramTec RK 87 Alumina, 99.8%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Maximum Service Temperature, Inert 1500 °C
2730 °F
CeramTec V 679 Alumina, 99.7%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Maximum Service Temperature, Inert 1500 °C
2730 °F
CeramTec AT 79 Alumina, 99.6%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.