Polymer Property : Thermal Conductivity = 201 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.550 - 29.0 W/m-K
3.82 - 201 BTU-in/hr-ft²-°F
Average value: 2.78 W/m-K Grade Count:72
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..