Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco 10 AS WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® 400 Wollastonite Chemically treated powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an .. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® M200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® MD1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ULTRAFIBRE® 30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ULTRAFIBRE® II Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |