Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 50.0 - 200 W/m-K | 347 - 1390 BTU-in/hr-ft²-°F | |
NanoAmor 50% Regular Single Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an.. |
|||
Thermal Conductivity | 50.0 - 200 W/m-K | 347 - 1390 BTU-in/hr-ft²-°F | |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Thermal Conductivity | 195 - 200 W/m-K | 1350 - 1390 BTU-in/hr-ft²-°F | x-y direction |
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | x-y direction |
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | |
MarkeTech Mo70Cu Moly/Copper Heat Sink Material MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit.. |
|||
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | |
MarkeTech W85Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
Thermal Conductivity | 190 - 200 W/m-K | 1320 - 1390 BTU-in/hr-ft²-°F | |
MarkeTech WCu15 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
Thermal Conductivity | 130 - 200 W/m-K | 902 - 1390 BTU-in/hr-ft²-°F | |
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-5S Alnico Magnetic Material |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-8S Alnico Magnetic Material |
|||
Thermal Conductivity | 160 - 200 W/m-K | 1110 - 1390 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 1370CS AlN Applications:replacement for 99.5 BeOcollector rodshelix supportswindowsFeatures: higher thermal conductivity than BeO at high temperatures.Information provided by Ceradyne Company |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-6S Alnico Magnetic Material |
|||
Thermal Conductivity | 10.0 - 200 W/m-K | 69.4 - 1390 BTU-in/hr-ft²-°F | |
Alliance A-2S Alnico Magnetic Material |