Polymer Property : Thermal Conductivity = 1.56 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 - 0.225 W/m-K
1.32 - 1.56 BTU-in/hr-ft²-°F
Average value: 0.202 W/m-K Grade Count:3
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..