Polymer Property : Thermal Conductivity = 0.347 BTU-in/hr-ft²-°F
Polymer Property :
Thermal Conductivity =
0.347 BTU-in/hr-ft²-°F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.0330
-
0.0500
W/m-K
0.229
-
0.347
BTU-in/hr-ft²-°F
ERG Aerospace Reticulated Vitreous Carbon (RVC)
Glass-like Carbon Foam