Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 0% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 10% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 20% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 20% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 20% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 20% cold reduction, 1120°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 20% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 30% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 40% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 40% cold reduction, 1120°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 40% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 50% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 50% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, plate after 1000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, plate after 16000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, plate after 4000 hours at 650°C (1200°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, plate after 4000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, plate after 8000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, plate after 8000 hours at 870°C (1600°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, plate, as annealed at 1025°C, rapid cooled Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® C276 Nickel Superalloy Bar Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special .. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® C276 Nickel Superalloy Sheet Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 40% cold reduction, 1010°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 50% cold reduction, 1120°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 10% cold reduction, 1120°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 10% cold reduction, 1175°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |
|||
Thermal Conductivity | 9.80 W/m-K | 68.0 BTU-in/hr-ft²-°F | RT |
Haynes 625 alloy, 40% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |