Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.790 W/m-K @Temperature 80.0 °C |
5.48 BTU-in/hr-ft²-°F @Temperature 176 °F |
Z Direction; ASTM C518 |
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | |
Schott N-LAF36 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | |
Schott N-LASF41 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | |
Schott N-LASF9 Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | |
Schott P-SF67 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | |
Schott N-LASF31a Glass Information Provided by SCHOTT North America, Inc. |
|||
Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | ASTM C518 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |
|||
Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | ASTM C518 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |