| Category | Ceramic , Glass |
| Manufacturer | Schott North America |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Schott N-LASF31a Glass.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 5.51 g/cc | 0.199 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Knoop Microhardness | 650 | 650 | .1/20 |
| Modulus of Elasticity | 126 GPa | 18300 ksi | |
| Poissons Ratio | 0.301 | 0.301 | |
| Shear Modulus | 48.0 GPa | 6960 ksi | calculated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 6.70 µm/m-°C <br>@Temperature -30.0 - 70.0 °C |
3.72 µin/in-°F <br>@Temperature -22.0 - 158 °F |
|
| 7.70 µm/m-°C <br>@Temperature 20.0 - 300 °C |
4.28 µin/in-°F <br>@Temperature 68.0 - 572 °F |
||
| Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
| Thermal Conductivity | 0.790 W/m-K | 5.48 BTU-in/hr-ft²-°F | |
| Transformation Temperature, Tg | 719 °C | 1330 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.883 <br>@Wavelength 587.6 nm |
1.883 <br>@Wavelength 587.6 nm |
n<sub>d</sub> |
| 1.88815 <br>@Wavelength 546.1 nm |
1.88815 <br>@Wavelength 546.1 nm |
n<sub>e</sub> | |
| Transmission, Visible | 84.2 % <br>@Thickness 10.0 mm,<br> Wavelength 380 nm |
84.2 % <br>@Thickness 0.394 in,<br> Wavelength 380 nm |
|
| 93.3 % <br>@Thickness 10.0 mm,<br> Wavelength 405 nm |
93.3 % <br>@Thickness 0.394 in,<br> Wavelength 405 nm |
||
| 97.4 % <br>@Thickness 10.0 mm,<br> Wavelength 460 nm |
97.4 % <br>@Thickness 0.394 in,<br> Wavelength 460 nm |
||
| 99.5 % <br>@Thickness 10.0 mm,<br> Wavelength 580 nm |
99.5 % <br>@Thickness 0.394 in,<br> Wavelength 580 nm |
||
| 99.6 % <br>@Thickness 10.0 mm,<br> Wavelength 700 nm |
99.6 % <br>@Thickness 0.394 in,<br> Wavelength 700 nm |
||
| IR Transmittance | 63.4 % <br>@Thickness 10.0 mm,<br> Wavelength 2500 nm |
63.4 % <br>@Thickness 0.394 in,<br> Wavelength 2500 nm |
|
| 99.2 % <br>@Thickness 10.0 mm,<br> Wavelength 1530 nm |
99.2 % <br>@Thickness 0.394 in,<br> Wavelength 1530 nm |
||
| UV Transmittance | 0.10 % <br>@Thickness 10.0 mm,<br> Wavelength 320 nm |
0.10 % <br>@Thickness 0.394 in,<br> Wavelength 320 nm |
|
| 12.3 % <br>@Thickness 10.0 mm,<br> Wavelength 334 nm |
12.3 % <br>@Thickness 0.394 in,<br> Wavelength 334 nm |
||
| 46.8 % <br>@Thickness 10.0 mm,<br> Wavelength 350 nm |
46.8 % <br>@Thickness 0.394 in,<br> Wavelength 350 nm |
||
| 76.4 % <br>@Thickness 10.0 mm,<br> Wavelength 370 nm |
76.4 % <br>@Thickness 0.394 in,<br> Wavelength 370 nm |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 2.3 | 2.3 | |
| Alkali Class, AR | 1.0 | 1.0 | |
| Stain Resistance Class, FR | 0.00 | 0.00 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| B | 1 | |
| Climatic Resistance Test CR | 1 | |
| HG | 2 | |
| K (10-6mm2/N) | 1.18 | |
| Phosphate Resistance PR | 1 | |
| T1013.0 (°C) | 720 | |
| T107.6 (°C) | 830 |