Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 55.3 W/m-K @Temperature 20.0 - 100 °C |
384 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck NRC® 3N5 (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Thermal Conductivity | 55.3 W/m-K @Temperature 20.0 - 100 °C |
384 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck NRC® 4N (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Thermal Conductivity | 55.3 W/m-K @Temperature 20.0 - 100 °C |
384 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck NRC® 4N5 (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Thermal Conductivity | 55.3 W/m-K @Temperature 20.0 - 100 °C |
384 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck NRC® 5N (UNS R05200) Electron Beam Melted Tantalum Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applicatio.. |
|||
Thermal Conductivity | 55.3 W/m-K @Temperature 20.0 - 100 °C |
384 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck NRC® Tantalum (UNS R05200) Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture di.. |
|||
Thermal Conductivity | 55.3 W/m-K @Temperature 20.0 - 100 °C |
384 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck Ultra 76 Alloy (Ta 2.5%W) Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low.. |