Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 Hard, 1.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 MH12, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 MH8, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H925 (H925) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.7Formability Ratio (bad Way).. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 1/2 Hard, 1.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 1.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard, 2.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 Hard Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way).. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Thermal Conductivity | 48.0 W/m-K @Temperature 85.0 °C |
333 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 116 Tin-Lead Solder Alloy General purpose solderInformation Provided by Indium Corporation |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H1050 (H1050) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
|||
Thermal Conductivity | 48.0 W/m-K | 333 BTU-in/hr-ft²-°F | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; H775 (H775) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |