Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 46.05 W/m-K

@Temperature 25.0 °C
319.6 BTU-in/hr-ft²-°F

@Temperature 77.0 °F