Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.22 W/m-K | 15.4 BTU-in/hr-ft²-°F | in-plane, ø80*3mm discs; ISO 22007-2 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |