Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, plate at RT after 0 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, plate at RT after 8000 hours at 650°C (1200°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 188 alloy, plate at RT after 8000 hours at 870°C (1600°F) Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 50% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 214® alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 15.9 W/m-K @Temperature 300 °C |
110 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316 Austenitic Stainless Steel, Annealed The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316L Austenitic Stainless Steel, 1/8 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316L Austenitic Stainless Steel, 3/4 Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316L Austenitic Stainless Steel, Annealed Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Thermal Conductivity | 15.9 W/m-K | 110 BTU-in/hr-ft²-°F | |
Eagle Brass 316L Austenitic Stainless Steel, Full Hardened Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a.. |
|||
Thermal Conductivity | 15.8 W/m-K @Temperature 50.0 °C |
110 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
ATI Allegheny Ludlum Ohmaloy® 30 Resistance Alloy Ohmaloy 30 alloy is a moderately magnetic, ductile stainless steel having extremely high electrical resistivity. In addition to imparting high electrical resistivity, the aluminum content in these .. |