Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.178 W/m-K | 1.24 BTU-in/hr-ft²-°F | |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch.. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT5005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding gradeMakroblend DP UT5005* provides an outstanding balance of low-temperature impact strength and flowability beside e.. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT5007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT5007* provides an outstanding balance of low-temperature impact strength and flow.. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis.. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c.. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch.. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® KU 2-7915 Polycarbonate + PBT, Impact Grade ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradeexcellent toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist.. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP 6015 Polycarbonate + PBT Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade. Makroblend DP 6015* provides an outstanding balance of low-temperature impact strength and excellent chemical .. |
|||
Thermal Conductivity | 0.179 W/m-K | 1.24 BTU-in/hr-ft²-°F | Melt |
Covestro Makroblend® DP UT6007 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT6007* offers an exceptional low-temperature impact strength, good flowability and.. |
|||
Thermal Conductivity | 0.178 W/m-K | 1.24 BTU-in/hr-ft²-°F | |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |