Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K20 Very Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K30-15 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K40-20 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K30-20 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |
|||
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |
|||
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K40-35 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |
|||
Thermal Conductivity | 0.0865 W/m-K | 0.600 BTU-in/hr-ft²-°F | ASTM E1530 |
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |