Polymer Property : Thermal Conductivity = 0.319 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
mean temp of 80°C; ASTM C 518
Zotefoams ZOTEK® F OSU Flexible PVDF Foam
Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and ..
Thermal Conductivity 0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
mean temp of 80°C; ASTM C 518
Zotefoams ZOTEK® F 30 PVDF Foam
Zotek® F 30 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..
Thermal Conductivity 0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
mean temp of 80°C; ASTM C 518
Zotefoams ZOTEK® F 35 PVDF Foam
Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..
Thermal Conductivity 0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9270 0.1 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea..
Thermal Conductivity 0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9280 0.1 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea..
Thermal Conductivity 0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9280 0.11 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea..
Thermal Conductivity 0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
DIN 52612
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea..