Thermal Properties Metric English Comments
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 1%
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 2%
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F

@Thickness 2.36 in
DIN EN 13164
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 1%
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 2%
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F

@Thickness 2.36 in
DIN EN 13164
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 1%
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 2%
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F

@Thickness 2.36 in
DIN EN 13164
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Thickness 50.0 mm,
Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F

@Thickness 1.97 in,
Temperature 68.0 °F
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
ISO 8301
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 1%
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 2%
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F

@Thickness 2.36 in
DIN EN 13164
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 1%
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 2%
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F

@Thickness 2.36 in
DIN EN 13164
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 1%
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
Moisture Content: 2%
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Temperature 20.0 °C
0.236 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Thermal Conductivity 0.0340 W/m-K

@Thickness 60.0 mm
0.236 BTU-in/hr-ft²-°F

@Thickness 2.36 in
DIN EN 13164
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Copyright © lookpolymers.com All Rights Reserved