Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 - 0.251 W/m-K | 1.59 - 1.74 BTU-in/hr-ft²-°F | |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Thermal Conductivity | 0.150 - 0.251 W/m-K | 1.04 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:11 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |