TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: ..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness,
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness,
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness,
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness,
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries ..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet
Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5),
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are ..
Thermal Conductivity 6.60 W/m-K
45.8 BTU-in/hr-ft²-°F
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G; other specific form/thickness entries are ..