Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 6.57 W/m-K @Temperature 600 °C |
45.6 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Zircar Refractory Composites RS-DA Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |