Polymer Property : Thermal Conductivity = 6.50 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 6.50 W/m-K
45.1 BTU-in/hr-ft²-°F
ASTM E 1530 & ASTM E 1461-01
Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma..