Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 17.9 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 17.9 W/m-K | 124 BTU-in/hr-ft²-°F | |
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils .. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 500 °C |
124 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
Thermal Conductivity | 17.9 W/m-K @Temperature 200 °C |
124 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |