Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 14.9 W/m-K | 103 BTU-in/hr-ft²-°F | |
Special Metals INCONEL® Alloy 600 A nickel-chromium alloy with good oxidation resistance at high temperatures and resistance to chloride-ion stress-corrosion cracking, corrosion by high-purity water, and caustic corrosion. Used for.. |
|||
Thermal Conductivity | 14.9 - 16.5 W/m-K | 103 - 115 BTU-in/hr-ft²-°F | after modified H900 heat treatment, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |