Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 13.4 W/m-K | 93.0 BTU-in/hr-ft²-°F | |
Goodfellow Nichrome®, Tophet A® Nickel 80 Chromium 20 Alloy Information provided by Goodfellow. |
|||
Thermal Conductivity | 13.4 W/m-K | 93.0 BTU-in/hr-ft²-°F | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t.. |
|||
Thermal Conductivity | 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |