Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, 1/2 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, 1/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, 3/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, Annealed Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, Extra Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, Extra Spring Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Eagle Brass 425 Tin Brass 2%, Spring Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Thermal Conductivity | 119 W/m-K | 828 BTU-in/hr-ft²-°F | |
Chicago Extruded Metals UNS C37700 Copper-Zinc-Lead Alloy Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, M30Information provided by Chicago Extruded Metals |