Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | >= 0.749 W/m-K | >= 5.20 BTU-in/hr-ft²-°F | ASTM C177 |
PolyOne Lubri-Tech™ SF-30CF/13T2S Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE/Silicone Lubricated
&n Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Thermal Conductivity | 0.749 W/m-K | 5.20 BTU-in/hr-ft²-°F | ASTM F433 |
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe.. |