Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.607 W/m-K | 4.21 BTU-in/hr-ft²-°F | ASTM F433 |
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |