POLYMER SEARCH
Polymer Property : Thermal Conductivity = 0.212 W/m-K
Polymer Property :
Thermal Conductivity =
0.212 W/m-K
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.212
W/m-K
1.47
BTU-in/hr-ft²-°F
ASTM C177
Quantum Polycarbonate 20% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics