Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.113 W/m-K @Temperature 600 °C |
0.784 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Sharadaa Ceramics Vacuum Formed Boards Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Thermal Conductivity | 0.113 W/m-K | 0.784 BTU-in/hr-ft²-°F | |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |