Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | 20 g/l; EN 12667 |
Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding High quality processingHigh strengthLow wasteFast moulding cycles |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9335 MG 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 3% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 4% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Temperature 30.0 °C |
0.243 BTU-in/hr-ft²-°F @Temperature 86.0 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Thickness 80.0 mm |
0.243 BTU-in/hr-ft²-°F @Thickness 3.15 in |
DIN EN 13164 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® T92.110 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 3% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 4% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Temperature 30.0 °C |
0.243 BTU-in/hr-ft²-°F @Temperature 86.0 °F |
|
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Thickness 80.0 mm |
0.243 BTU-in/hr-ft²-°F @Thickness 3.15 in |
DIN EN 13164 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 3% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 4% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Thickness 80.0 mm |
0.243 BTU-in/hr-ft²-°F @Thickness 3.15 in |
DIN EN 13164 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Thickness 50.0 mm, Temperature 30.0 °C |
0.243 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature 86.0 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 3% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 4% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Temperature 30.0 °C |
0.243 BTU-in/hr-ft²-°F @Temperature 86.0 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 3% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 4% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Temperature 30.0 °C |
0.243 BTU-in/hr-ft²-°F @Temperature 86.0 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Thickness 80.0 mm |
0.243 BTU-in/hr-ft²-°F @Thickness 3.15 in |
DIN EN 13164 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 3% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | Moisture Content: 4% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Temperature 30.0 °C |
0.243 BTU-in/hr-ft²-°F @Temperature 86.0 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K @Thickness 80.0 mm |
0.243 BTU-in/hr-ft²-°F @Thickness 3.15 in |
DIN EN 13164 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0350 W/m-K | 0.243 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |