Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 1% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 2% |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Temperature 20.0 °C |
0.236 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Thickness 60.0 mm |
0.236 BTU-in/hr-ft²-°F @Thickness 2.36 in |
DIN EN 13164 |
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 1% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 2% |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Temperature 20.0 °C |
0.236 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Thickness 60.0 mm |
0.236 BTU-in/hr-ft²-°F @Thickness 2.36 in |
DIN EN 13164 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 1% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 2% |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Thickness 60.0 mm |
0.236 BTU-in/hr-ft²-°F @Thickness 2.36 in |
DIN EN 13164 |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Thickness 50.0 mm, Temperature 20.0 °C |
0.236 BTU-in/hr-ft²-°F @Thickness 1.97 in, Temperature 68.0 °F |
|
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | ISO 8301 |
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 1% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 2% |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Temperature 20.0 °C |
0.236 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Thickness 60.0 mm |
0.236 BTU-in/hr-ft²-°F @Thickness 2.36 in |
DIN EN 13164 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 1% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 2% |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Temperature 20.0 °C |
0.236 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Thickness 60.0 mm |
0.236 BTU-in/hr-ft²-°F @Thickness 2.36 in |
DIN EN 13164 |
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 1% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K | 0.236 BTU-in/hr-ft²-°F | Moisture Content: 2% |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Temperature 20.0 °C |
0.236 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Thermal Conductivity | 0.0340 W/m-K @Thickness 60.0 mm |
0.236 BTU-in/hr-ft²-°F @Thickness 2.36 in |
DIN EN 13164 |
BASF Styrodur® 3035 CN Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |