Thermal Properties Metric English Comments
CTE, linear 117 - 171 µm/m-°C
65.0 - 95.0 µin/in-°F
Average value: 150 µm/m-°C Grade Count:15
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
CTE, linear 50.0 - 171 µm/m-°C

@Temperature 25.6 - 300 °C
27.8 - 95.0 µin/in-°F

@Temperature 78.0 - 572 °F
Average value: 110 µm/m-°C Grade Count:11
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..