Thermal Properties Metric English Comments
CTE, linear 49.0 - 137 µm/m-°C
27.2 - 76.1 µin/in-°F
Average value: 75.3 µm/m-°C Grade Count:10
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum and ..