Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 101 - 121 µm/m-°C @Temperature 20.0 °C |
56.0 - 67.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |