Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 48.0 - 74.4 µm/m-°C | 26.7 - 41.3 µin/in-°F | Average value: 65.6 µm/m-°C Grade Count:26 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |