Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 20.0 - 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
11.1 - 25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Lexan® LCG2007 PC (Asia Pacific) |
|||
CTE, linear | 9.00 - 45.0 µm/m-°C | 5.00 - 25.0 µin/in-°F | Average value: 20.0 µm/m-°C Grade Count:4 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
CTE, linear | 20.0 - 45.0 µm/m-°C | 11.1 - 25.0 µin/in-°F | Average value: 32.0 µm/m-°C Grade Count:10 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
CTE, linear | 27.0 - 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.0 - 25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL S100G20 PPE+PS (Asia Pacific) |
|||
CTE, linear | 28.0 - 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.6 - 25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump.. |
|||
CTE, linear | 28.0 - 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.6 - 25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics Noryl GFN2L PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear | 28.0 - 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.6 - 25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GFN2L PPE+PS (Asia Pacific) PPE+PS GF20%, hydrolytic stability |
|||
CTE, linear | 25.0 - 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
13.9 - 25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL NC212 PPE+HIPS (Asia Pacific) |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulat.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP41S-1HTND Non-Drip, High Performance Epoxy Adhesive Description: Master Bond EP41S-1HTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a 100 to 30 mix ratio by weight and its viscosity is a smooth pas.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System Master Bond Polymer System EP46HT-2MED is a two component medical grade epoxy system for high performance structural bonding and casting suitable for applications where resistance to temperatures fr.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or .. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
CTE, linear | 40.0 - 45.0 µm/m-°C | 22.2 - 25.0 µin/in-°F | |
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used.. |
|||
CTE, linear | 36.0 - 45.0 µm/m-°C | 20.0 - 25.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
CTE, linear | 28.0 - 45.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
15.6 - 25.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL PX2934 PPE+PS (Asia Pacific) PPE+PS GF20% High Heat Non-FR |